From: Influence of surface treatment and curing mode of resin composite cements on fibroblast behavior
Curing mode | Surface treatment | MLA | RUN |
---|---|---|---|
Autopolymerization | Oxygen inhibition layer | 25.7 ± 20.2Aa | 46.6 ± 13.3Aa |
Polished | 86.0 ± 22.4BCa | 85.6 ± 12.9BCa | |
Scaler | 88.2 ± 32.7BCa | 75.0 ± 16.9Ba | |
Light-curing | Oxygen inhibition layer | 68.7 ± 26.5Ba | 93.2 ± 25.2BDb |
Polished | 87.8 ± 11.8BCa | 110.0 ± 23.2CDa | |
Scaler | 105.0 ± 18.6Ca | 111.9 ± 31.4Da |