From: Release kinetics of the model protein FITC-BSA from different polymer-coated bovine bone substitutes

RESOMER R 203 H (Boehringer Ingelheim), Lot.: 1038461, Poly (DL-lactide), inherent viscosity: 0.25–0.35 dl/g, mean molecular weight: 18–28 tsd Dalton.

RESOMER RG 503 H (Boehringer Ingelheim), Lot.: 1037323, Poly (DL-lactide-coglycolide), acid terminated, lactide/glycolide ratio = 50:50, inherent viscosity: 0.32–0.44 dl/g, mean molecular weight: 24–38 tsd Dalton.

RESOMER RG 504 H (Sigma Aldrich), Lot.: STBD1648V, Poly (DL-lactide-coglycolide), acid terminated, lactide/glycolide ratio = 50:50, inherent viscosity: 0.45–0.6 dl/g, mean molecular weight: 38–54 tsd Dalton.

RESOMER RG 505 (Sigma Aldrich), Lot.: STBD7078V, Poly (DL-lactide-coglycolide), ester terminated, lactide/glycolide ratio = 50:50, inherent viscosity: 0.61–0.74 dl/g, mean molecular weight: 54–69 tsd Dalton.

RESOMER L 206 S (Sigma Aldrich), Lot.: STBD8857V, Poly (DL-lactide), ester terminated, inherent viscosity: 0.8–1,2 dl/g, mean molecular weight: N/A.