Skip to main content

Table 2 Failure mode of ProRoot MTA (MTA), Biodentine (BD), ChemFil rock (GIC) and X-trabase (composite resin) in combination with Futurabond DC (CR) on dentine after 2 d, 7 d and 14 d

From: Shear bond strength of Biodentine, ProRoot MTA, glass ionomer cement and composite resin on human dentine ex vivo

sample no. MTA 2 d MTA 7 d MTA 14 d BD 2 d BD 7 d BD 14 GIC 2 d GIC 7 d GIC 14 d CR 2 d CR 7 d CR 14 d
1 1 1 1 1 1 1 2 2 2 1 1 1
2 1 1 1 1 1 1 2 2 2 1 1 1
3 1 1 2 1 1 1 2 2 2 1 1 1
4 1 1 2 1 2 2 2 2 2 1 1 1
5 1 1 2 1 2 2 2 2 2 1 1 1
6 1 1 2 1 2 2 2 2 2 3 1 3
7 1 1 3 1 2 2 2 2 2 3 1 3
8 1 3 3 2 2 2 2 2 2 3 1 3
9 1 3 3 2 2 2 2 3 2 3 1 3
10 1 3 3 2 2 2 2 3 2 3 1 3
  1. 1 = adhesive failure mode that occurred at the filling material and dentine interface.
  2. 2 = cohesive failure mode within the filling material.
  3. 3 = mixed failure mode.